Abstract: A method for manufacturing a grain-oriented electrical steel sheet, according to one embodiment of the present invention, comprises the steps of: hot rolling a slab so as to manufacture a hot rolled sheet, the slab comprising, by wt%, 2.5-4.0% of Si, 0.03-0.09% of C, 0.015-0.040% of Al, 0.04-0.15% of Mn, 0.01% or less of S (excluding 0%), 0.002-0.012% of N, 0.01-0.05% of Sb, 0.03-0.1% of Sn, 0.05-0.2% of Cr and the balance of Fe and inevitable impurities; cold rolling the hot rolled sheet so as to manufacture a cold rolled sheet; performing primary recrystallization annealing on the cold rolled sheet; and performing secondary recrystallization annealing on the steel sheet having undergone primary recrystallization annealing.
| # | Name | Date |
|---|---|---|
| 1 | 202417052443-TRANSLATIOIN OF PRIOIRTY DOCUMENTS ETC. [09-07-2024(online)].pdf | 2024-07-09 |
| 2 | 202417052443-STATEMENT OF UNDERTAKING (FORM 3) [09-07-2024(online)].pdf | 2024-07-09 |
| 3 | 202417052443-REQUEST FOR EXAMINATION (FORM-18) [09-07-2024(online)].pdf | 2024-07-09 |
| 4 | 202417052443-PROOF OF RIGHT [09-07-2024(online)].pdf | 2024-07-09 |
| 5 | 202417052443-POWER OF AUTHORITY [09-07-2024(online)].pdf | 2024-07-09 |
| 6 | 202417052443-NOTIFICATION OF INT. APPLN. NO. & FILING DATE (PCT-RO-105-PCT Pamphlet) [09-07-2024(online)].pdf | 2024-07-09 |
| 7 | 202417052443-FORM 18 [09-07-2024(online)].pdf | 2024-07-09 |
| 8 | 202417052443-FORM 1 [09-07-2024(online)].pdf | 2024-07-09 |
| 9 | 202417052443-DECLARATION OF INVENTORSHIP (FORM 5) [09-07-2024(online)].pdf | 2024-07-09 |
| 10 | 202417052443-COMPLETE SPECIFICATION [09-07-2024(online)].pdf | 2024-07-09 |
| 11 | 202417052443-FORM 3 [10-10-2024(online)].pdf | 2024-10-10 |