Abstract: Provided is a Cr-Ni alloy tube in which the tensile yield stress YSLT and the compressive yield stress YSLC in the tube axial direction of the Cr-Ni alloy tube and the tensile yield stress YSHT of a test piece after high-frequency induction heating and quenching satisfy [0.80 = YSLC/YSLT < 0.95], [YS HT - 0.24 × YSLT = 50.0], and [YSLT = 443 × YSLT/YSLC + 2.28 × YSHT - 350], the test piece being collected from a thickness center position of the Cr-Ni alloy tube so that the longitudinal direction of the test piece is parallel to the tube axial direction.
| # | Name | Date |
|---|---|---|
| 1 | 202517084068-STATEMENT OF UNDERTAKING (FORM 3) [04-09-2025(online)].pdf | 2025-09-04 |
| 2 | 202517084068-REQUEST FOR EXAMINATION (FORM-18) [04-09-2025(online)].pdf | 2025-09-04 |
| 3 | 202517084068-PROOF OF RIGHT [04-09-2025(online)].pdf | 2025-09-04 |
| 4 | 202517084068-POWER OF AUTHORITY [04-09-2025(online)].pdf | 2025-09-04 |
| 5 | 202517084068-FORM 18 [04-09-2025(online)].pdf | 2025-09-04 |
| 6 | 202517084068-FORM 1 [04-09-2025(online)].pdf | 2025-09-04 |
| 7 | 202517084068-FIGURE OF ABSTRACT [04-09-2025(online)].pdf | 2025-09-04 |
| 8 | 202517084068-DECLARATION OF INVENTORSHIP (FORM 5) [04-09-2025(online)].pdf | 2025-09-04 |
| 9 | 202517084068-COMPLETE SPECIFICATION [04-09-2025(online)].pdf | 2025-09-04 |