Abstract: A nanocrystal alloy ribbon is provided. According to this method for manufacturing a nanocrystal alloy ribbon, when an amorphous alloy ribbon is contacted with a heating body and heated, the heating body is heated to a heating temperature Ta of Tx1+80? or more and Tx1+230? or less, wherein Tx1? is the bcc Fe crystallization onset temperature of the amorphous alloy ribbon measured at a temperature-increase rate of 20 K/min.
| # | Name | Date |
|---|---|---|
| 1 | 202437082007-TRANSLATIOIN OF PRIOIRTY DOCUMENTS ETC. [28-10-2024(online)].pdf | 2024-10-28 |
| 2 | 202437082007-STATEMENT OF UNDERTAKING (FORM 3) [28-10-2024(online)].pdf | 2024-10-28 |
| 3 | 202437082007-REQUEST FOR EXAMINATION (FORM-18) [28-10-2024(online)].pdf | 2024-10-28 |
| 4 | 202437082007-PRIORITY DOCUMENTS [28-10-2024(online)].pdf | 2024-10-28 |
| 5 | 202437082007-POWER OF AUTHORITY [28-10-2024(online)].pdf | 2024-10-28 |
| 6 | 202437082007-FORM 18 [28-10-2024(online)].pdf | 2024-10-28 |
| 7 | 202437082007-FORM 1 [28-10-2024(online)].pdf | 2024-10-28 |
| 8 | 202437082007-DRAWINGS [28-10-2024(online)].pdf | 2024-10-28 |
| 9 | 202437082007-DECLARATION OF INVENTORSHIP (FORM 5) [28-10-2024(online)].pdf | 2024-10-28 |
| 10 | 202437082007-COMPLETE SPECIFICATION [28-10-2024(online)].pdf | 2024-10-28 |
| 11 | 202437082007-FORM 3 [11-04-2025(online)].pdf | 2025-04-11 |
| 12 | 202437082007-Proof of Right [21-04-2025(online)].pdf | 2025-04-21 |