Abstract: There are provided a method for manufacturing a solid electrolyte battery and a solid electrolyte battery, each of which can reduce the number of films and can obtain excellent performance. This method for manufacturing a solid electrolyte battery has a laminate formation step of forming a laminate in which a lower collector layer 12, an interlayer 13, and an upper collector layer 14 are laminated in this order on a substrate 11 and a step of applying a voltage to the laminate.
NA
| # | Name | Date |
|---|---|---|
| 1 | 7699-delnp-2011-GPA.pdf | 2012-03-27 |
| 2 | 7699-delnp-2011-Form-5.pdf | 2012-03-27 |
| 3 | 7699-delnp-2011-Form-3.pdf | 2012-03-27 |
| 4 | 7699-delnp-2011-Form-2.pdf | 2012-03-27 |
| 5 | 7699-delnp-2011-Form-18.pdf | 2012-03-27 |
| 6 | 7699-delnp-2011-Form-1.pdf | 2012-03-27 |
| 7 | 7699-delnp-2011-Drawings.pdf | 2012-03-27 |
| 8 | 7699-delnp-2011-Description (Complete).pdf | 2012-03-27 |
| 9 | 7699-delnp-2011-Correspondence Others.pdf | 2012-03-27 |
| 10 | 7699-delnp-2011-Claims.pdf | 2012-03-27 |
| 11 | 7699-delnp-2011-Abstract.pdf | 2012-03-27 |
| 12 | 7699-delnp-2011-Form-3-(23-04-2012).pdf | 2012-04-23 |
| 13 | 7699-delnp-2011-Correspondence-others-(23-04-2012).pdf | 2012-04-23 |
| 14 | 7699-delnp-2011-Form-3-(14-06-2012).pdf | 2012-06-14 |
| 15 | 7699-delnp-2011-Correspondence-Others-(14-06-2012).pdf | 2012-06-14 |
| 16 | 7699-delnp-2011-Form-3-(24-01-2014).pdf | 2014-01-24 |
| 17 | 7699-delnp-2011-Correspondence-Others-(24-01-2014).pdf | 2014-01-24 |
| 18 | 7699-DELNP-2011-FER.pdf | 2017-05-09 |
| 19 | 7699-DELNP-2011-AbandonedLetter.pdf | 2018-02-01 |
| 1 | search7699_28-04-2017.pdf |