Abstract: Disclosed is a method for adequately producing a high-performance optical material (such as a lens) composed of a polyurethane resin, which optical material is clear and colorless, while having no strain. In this method, the optical material is produced without causing cord or white turbidity by polymerizing a polymerizable composition characterized by containing 10-300 ppm of moisture and composed of a polythiol compound and a polyiso(thio )cyanate compound.
CLIAMS:Please find the attached file ,TagSPECI:Please find the attached file
| # | Name | Date |
|---|---|---|
| 1 | F2.pdf | 2014-05-22 |
| 2 | 1051-KOLNP-2014-(05-11-2014)-FORM-1.pdf | 2014-11-05 |
| 3 | 1051-KOLNP-2014-(03-08-2015)-CORRESPONDENCE.pdf | 2015-08-03 |
| 4 | 1051-KOLNP-2014-(03-08-2015)-ANNEXURE TO FORM 3.pdf | 2015-08-03 |
| 5 | 1051-KOLNP-2014-(03-09-2015)-CORRESPONDENCE.pdf | 2015-09-03 |
| 6 | 1051-KOLNP-2014-(03-09-2015)-ANNEXURE TO FORM 3.pdf | 2015-09-03 |
| 7 | 1051-KOLNP-2014-FER.pdf | 2018-06-29 |
| 8 | 1051-KOLNP-2014-AbandonedLetter.pdf | 2024-06-18 |
| 1 | TACD_29-06-2018.pdf |