Abstract

Present disclosure discloses a method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process is disclosed. The method includes addition of a bottom batch into a furnace shell and charging hot metal into the furnace shell. The hot metal comprises sulphur (S) composition in wt% ranging between 0.005%-0.01%. Further, the method includes blowing a predetermined quantity of oxygen into the furnace shell at a predetermined flow rate, which is followed by arcing in the furnace shell for melting and to increase temperature to a tapping temperature. Furthermore, the method includes tapping steel out of the furnace shell. Tapped steel comprises composition of Nitrogen (N) in range of 30 ppm to 40 ppm.

Applicants

1
India
TATA STEEL LIMITED Jamshedpur – 831001, Jharkhand, India

Inventors

7
India
Prakash GuptaC/o., TATA STEEL LIMITED, Jamshedpur – 831 001, Jharkhand, India
India
Vimal TiwariC/o., TATA STEEL LIMITED, Jamshedpur – 831 001, Jharkhand, India
India
Pritish NayakC/o., TATA STEEL LIMITED, Jamshedpur – 831 001, Jharkhand, India
India
Tapas Kumar RoyC/o., TATA STEEL LIMITED, Jamshedpur – 831 001, Jharkhand, India
India
Balakrishnan V.C/o., TATA STEEL LIMITED, Jamshedpur – 831 001, Jharkhand, India
India
Harpanahalli MaheshbabuC/o., TATA STEEL LIMITED, Jamshedpur – 831 001, Jharkhand, India
India
Santosh KakarlapudiC/o., TATA STEEL LIMITED, Jamshedpur – 831 001, Jharkhand, India

Specification

Show full textCollapse

TECHNICAL FIELD Present disclosure in general relates to a field of manufacturing. Particularly, but not exclusively, the present disclosure relates to a method of manufacturing steel through 5 CONverter ARCing (CONARC) steel making process. Further embodiments of the present disclosure discloses a method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process. BACKGROUND OF THE DISCLOSURE 10 CONverter ARCing (CONARC) steel making process is combination of basic oxygen furnace (BOF) process and electric arcing furnace (EAF) process. BOF process is employed for decarburization of hot metal and the EAF process is employed for melting of solid inputs materials. The CONARC process aims to use large quantity of hot metal in the EAF part, 15 which minimises electrical energy consumption and maximizes productivity. Generally, CONARC furnace includes two furnace shells, rotating electrode structures, a transformer for supplying electricity to the furnace shells and an oxygen lance system. The two furnace shells are used interchangeably. That is, one shell can operate either as a BOF 20 shell or as an EAF shell at a particular time. In other words, if one furnace shell is operating as BOF shell, the other shell has to operate as the EAF shell. Apart from the advantages catered by the CONARC process, the major problem associated with the CONARC process is that, nitrogen content in the steel which is about 40 to 50 ppm. Such high content Nitrogen in the steel, leads to formation of blowholes; precipitation of one or more nitride compounds; 25 and the solidification of nitrogen in interstitial solid solution. High nitrogen content may also result in inconsistent mechanical properties in hot-rolled products, embrittlement of the heat affected zone (HAZ) of welded steels, and poor cold formability. Nitrogen can result in strain ageing and reduced ductility of cold-rolled and annealed LCAK steels. 30 The present disclosure is directed to overcome one or more limitations stated above or any other limitation associated with the conventional arts. SUMMARY OF THE DISCLOSURE 35 One or more shortcomings of the conventional techniques are overcome by a method as disclosed and additional advantages are provided through the method as described in the present disclosure. 3 Additional features and advantages are realized through the technique of the present disclosure. Other embodiments and aspects of the disclosure are described in detail herein and are considered a part of the claimed disclosure. 5 In one non-limiting embodiment of the present disclosure, a method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process is disclosed. The method includes addition of a bottom batch into a furnace shell and charging hot metal into the furnace shell. The hot metal comprises sulphur (S) composition in wt% 10 ranging between 0.005%-0.01%. Further, the method includes blowing a predetermined quantity of oxygen into the furnace shell at a predetermined flow rate, which is followed by arcing in the furnace shell for melting and to increase temperature to a tapping temperature. Furthermore, the method includes tapping steel out of the furnace shell. Tapped steel comprises composition of Nitrogen (N) in range of 30 ppm to 40 ppm. 15 In an embodiment, the bottom batch comprises calcined lime or calcined dolomite, direct reduced iron (DRI) and Cold briquetted iron (CBI). In an embodiment, blowing of oxygen is performed by a water cooled oxygen lance. In an embodiment, the predetermined flow rate of oxygen is 180-210 Nm3 /min and the predetermined quantity of oxygen ranges between 5000-6000 Nm3 . 20 In an embodiment, the method includes charging direct reduced iron (DRI) and Cold briquetted iron (CBI) into the furnace shell during blowing of oxygen. In an embodiment, the method includes comprising charging direct reduced iron (DRI), Cold briquetted iron (CBI), calcined lime and calcined dolomite into the furnace shell, during arcing. 25 In an embodiment, the tapping temperature ranges between 1620 °C -1640 °C. In another non-limiting embodiment of the present disclosure, steel manufactured by the method of the present disclosure is disclosed. The steel includes an alloying composition of Carbon (C) of 0.050, Phosphorous (P) of 0.015, Nitrogen (N) ranging between 30 ppm to 40 ppm, Silicon (Si) of 0.005 and balance being substantially iron and incidental impurities. 4 It is to be understood that the aspects and embodiments of the disclosure described above may be used in any combination with each other. Several of the aspects and embodiments may be combined together to form a further embodiment of the disclosure. 5 The foregoing summary is illustrative only and is not intended to be in any way limiting. In addition to the illustrative aspects, embodiments, and features described above, further aspects, embodiments, and features will become apparent by reference to the drawings and the following detailed description. 10 BRIEF DESCRIPTION OF THE ACCOMPANYING FIGURES The novel features and characteristics of the disclosure are set forth in the appended description. The disclosure itself, however, as well as a preferred mode of use, further objectives and advantages thereof, will best be understood by reference to the following 15 detailed description of an illustrative embodiment when read in conjunction with the accompanying figures. One or more embodiments are now described, by way of example only, with reference to the accompanying figures wherein like reference numerals represent like elements and in which: 20 Figure. 1 illustrates a schematic view of a CONverter ARCing (CONARC) steel making system, in accordance with an embodiment of the present disclosure. Figure. 2 is a flow chart of a method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process, in accordance with an 25 embodiment of the present disclosure. The figures depict embodiments of the disclosure for purposes of illustration only. One skilled in the art will readily recognize from the following description that alternative embodiments of the methods illustrated herein may be employed without departing from the 30 principles of the disclosure described herein. DETAILED DESCRIPTION The foregoing has broadly outlined the features and technical advantages of the present 35 disclosure in order that the detailed description of the disclosure that follows may be better understood. Additional features and advantages of the disclosure will be described hereinafter which form the subject of the description of the disclosure. It should also be realized by those 5 skilled in the art that such equivalent configuration of the system does not depart from the scope of the disclosure. The novel features which are believed to be characteristic of the disclosure, advantages will be better understood from the following description when considered in connection with the accompanying figures. It is to be expressly understood, 5 however, that each of the figures is provided for the purpose of illustration and description only and is not intended as a definition of the limits of the present disclosure. In the present document, the word "exemplary" is used herein to mean "serving as an example, instance, or illustration." Any embodiment or implementation of the present subject 10 matter described herein as "exemplary" is not necessarily to be construed as preferred or advantageous over other embodiments. While the disclosure is susceptible to various modifications and alternative forms, specific embodiments thereof have been shown by way of example in the drawings and will be 15 described in detail below. It should be understood, however, that it is not intended to limit the disclosure to the forms disclosed, but on the contrary, the disclosure is to cover all modifications, equivalents, and alternative falling within the spirit and the scope of the disclosure. 20 The terms “comprises”, “comprising”, or any other variations thereof, are intended to cover a non-exclusive inclusion, such that a method that comprises a list of acts does not include only those acts but may include other acts not expressly listed or inherent to such method. In other words, one or more acts in a method proceeded by “comprises… a” does not, without more constraints, preclude the existence of other acts or additional acts in the method. 25 Embodiments of the present disclosure discloses a method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process. Steel manufactured by conventional CONARC steel making process nitrogen content in the steel which is about 40 to 50 ppm. Such high content Nitrogen in the steel, leads to formation of blowholes; precipitation of one or more nitride compounds; and the solidification of nitrogen 30 in interstitial solid solution. High nitrogen content may also result in inconsistent mechanical properties in hot-rolled products, embrittlement of the heat affected zone (HAZ) of welded steels, and poor cold formability. Nitrogen can result in strain ageing and reduced ductility of cold-rolled and annealed steels, which is undesired. 6 In the method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process, the method includes addition of a bottom batch into a furnace shell. Further, the method includes charging a predetermined quantity of a hot metal into the furnace shell. The hot metal comprises sulphur (S) composition in wt% ranging 5 between 0.005%-0.01%. Further, the method includes blowing a predetermined quantity of oxygen into the furnace shell at a predetermined flow rate and arcing the furnace shell for melting and to increase temperature to a tapping temperature. Furthermore, the method includes tapping the steel out of the furnace shell. The steel obtained by the method of present disclosure includes Nitrogen in the range of 30 ppm to 40 ppm. 10 The present disclosure provides the following paragraphs which describe the present disclosure with reference to Figures. 1 and 2. In the figures, the same element or elements which have same functions are indicated by the same reference signs. In the following detailed description, embodiments of the disclosure are explained with 15 reference to accompanying figures that form a part hereof, and in which are shown by way of illustration specific embodiments in which the disclosure may be practiced. These embodiments are described in sufficient detail to enable those skilled in the art to practice the disclosure, and it is to be understood that other embodiments may be utilized and that changes may be made without departing from the scope of the present disclosure. The 20 following description is, therefore, not to be taken in a limiting sense. Figure. 1 illustrates a schematic view of a CONverter ARCing (CONARC) steel making system (100), in accordance with an embodiment of the present disclosure. The system (100) may include a pair of furnace shells (102), which may be movably supported by a support column (101). During operation, position of the pair of furnace shells (102) may be changed 25 based on the operation to be performed during steel making process. Further, the system (100) may include an oxygen blowing lance for blowing oxygen into the furnace shell (102). Furthermore, the system (100) may include a plurality of electrodes (104), which may be selectively lowered into the furnace shell (102) to perform arcing. To manufacture the steel, one of the pair of furnace may be added with a bottom batch, which 30 may include calcined lime or calcined dolomite, direct reduced iron (DRI) and Cold briquetted iron (CBI). Upon adding the bottom batch, de-sulphurised hot metal may be charged into the furnace shell (102). Upon charging the hot metal, oxygen may be blown into 7 the furnace shell (102), along with further addition of calcined lime and calcined dolomite may be added to carryout decarburization and oxidation to remove impurities such as C, Si, P, Mn and the like in the hot metal. Once oxygen blowing is completed, the furnace shell (102) may be positioned for lowering the electrodes (104) into the furnace shell (102) to perform 5 arcing process. Arcing causes melting of DRI and CBI, calcined lime or calcined dolomite and increase temperature to a tapping temperature, which may range between 1620 °C -1640 °C. The steel obtained includes composition of Nitrogen (N) in range of 30 ppm to 40 ppm. Henceforth, the present disclosure is explained with the help of flow chart for a method for 10 controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process. However, such exemplary embodiments should not be construed as limitations of the present disclosure since the method may be used for manufacturing other types of steel where such need arises. A person skilled in the art may envisage various such embodiments without deviating from scope of the present disclosure. 15 Figure. 2 is a flowchart depicting a method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process. The method aids in obtaining steel comprising Nitrogen in the range of 30 pm to 40 ppm, thereby improving properties and quality of the steel obtained. Further, the method of the present disclosure uses 20 raw materials such as calcined lime or calcined dolomite, direct reduced iron (DRI) and Cold briquetted iron (CBI) Nitrogen aids in obtaining the steel with less Nitrogen content. The order in which the method is described is not intended to be construed as a limitation, and any there may be some optional steps in between. Additionally, individual blocks may be deleted from the methods without departing from the scope of the subject matter described herein. 25 At block 201, a bottom batch may be added into a furnace shell (102). The furnace shell (101) may possess hot heel of predefined quantity on to the bottom may be added into the furnace shell (102). In an embodiment, the bottom batch may include calcined lime or calcined dolomite, direct reduced iron (DRI) and Cold briquetted iron (CBI). Nitrogen content in the calcined lime ranges between 300-400 ppm, in the calcined dolomite it ranges 30 between 400-500 ppm, in the DRI it ranges between 300-400 ppm and in the CBI it ranges between 600-700 ppm. The quantity of bottom batch depends on quantity of the hot metal charged into the furnace shell (102). Upon adding the bottom batch, as seen in block 202, the method may include charging hot metal into the furnace shell (102). The hot metal includes sulphur (S) composition in wt% ranging between 0.005%-0.01%. That is, the hot metal is de- 8 sulphurised before charging into the furnace shell (102). The sulphur (S) of this composition aids in effective absorption and desorption of Nitrogen (N), as sulphur (S) and oxygen (O) is the surface-active element in steel, presence of high quantity of surface-active elements not only retard the absorption of nitrogen (N) from atmosphere but also desorption of nitrogen 5 (N) from melt. At block 203, the method includes blowing of a predetermined quantity of oxygen into the furnace shell (102) at a predetermined flow rate. In an embodiment, blowing of oxygen is performed by a water cooled oxygen lance (103), with the predetermined flow rate may be 180-210 Nm3 /min and the predetermined quantity ranging between 5000-6000 Nm3 . In an 10 embodiment, the flow rate and quantity of oxygen indicative only and the same may vary and depends on quantity of hot metal charged into the furnace shell (102). During, blowing of oxygen calcined lime and calcined dolomite, DRI and CBI may be added to carryout decarburization and remove impurities such as C, Si, P, Mn and the like in the hot metal. Reactions occurring during blowing of oxygen is depicted below: 15 During the oxygen blowing period in CONARC furnace, impurities like Si, Mn and P which are present in hot metal get oxidised and forms SiO2, MnO, P2O5 and joins the slag. Si + O2 = SiO2……………………(1) Mn+1/2O2 = MnO…………………………………..(2) 2P + 5O2 = P2O5 …….…………………………………(3) 20 Silicon and phosphorous are removed with the help of added flux, as the slag is formed it holds the impurities. 3CaO + P2O5 = 3CaO.P2O5 ………………….(4) 2CaO + SiO2 = 2CaO.SiO2……………………(5) Once the impurities Si, Mn, P get oxidised during initial blowing period, Carbon starts 25 getting oxidised and joins the exit gas. C (s) + O2 (g) = CO2 (g)……………………………..(6) 2CO (g) + O2 (g) = 2CO2(g)………………………..(7) Further, during blowing of oxygen, direct reduced iron (DRI) and Cold briquetted iron (CBI) calcined lime, calcined dolomite may be charged into the furnace shell (102). The DRI and 30 CBI acts as coolant to control temperature inside the furnace shell (102). 9 Upon blowing of oxygen into the furnace shell (102), at block 204 the method includes arcing the furnace shell (102). Arcing is performed through electrodes (104) by using electrical energy. Arcing causes melting of calcined lime, calcined dolomite, DRI and CBI and increase temperature to a tapping temperature, which may range between 1620 °C -1640 5 °C. In an embodiment, Further, during arcing, calcined lime, calcined dolomite, DRI and CBI may be added achieve required tapping weight. Upon achieving the required tapping temperature and the tapping weight, the arcing process may be halted and steel may be tapped from the furnace shell (102) [as seen in block 205]. The tapped steel from the furnace shell (102) obtained through the method of the present disclosure, comprises composition of 10 Nitrogen (N) in range of 30 ppm to 40 ppm. The steel obtained with composition of Nitrogen (N) in range of 30 ppm to 40 ppm, is free of blowholes, no precipitation of one or more nitride compounds and no solidification of nitrogen in interstitial solid solution. Further, the steel possess good mechanical properties in hot-rolled products, exhibits no embrittlement of the heat affected zone (HAZ) of welded 15 steels, and good cold formability. Example: Experiments have been conducted by manufacturing the steel through CONverter ARCing (CONARC) steel making process through a method of the present disclosure. Hot heel quantity of 25 Ton was maintained in the furnace shell (102). A bottom batch has been added 20 into the furnace shell (102). The bottom batch includes 3 Ton lime, 10 Ton DRI and 5 Ton CBI. Upon adding the bottom batch, 135 Tons of desulphurized hot metal is charged into the furnace shell (102), where the desulphurized hot metal includes sulphur (S) composition in wt% ranging between 0.005%-0.01%. Upon charging the hot metal, oxygen was blown through water cooled top lance at the flow rate of 180-210 Nm3/min with addition of 3 Ton 25 lime and 3 Ton calcined dolomite. As the oxidation of impurities is exothermic in nature, coolants in the form of 15 Ton DRI and 10 Ton CBI was added to control the temperature inside of furnace. Total quantity of blown oxygen was 5000-6000 Nm3. Upon blowing of oxygen, electrodes (104) were lowered along with 30 Ton DRI and 25 Ton CBI, 3 Ton lime and 2 Ton dolomite. Arcing causes melting of DRI and CBI to achieve target tapping weight 30 and tapping temperature. During arcing, oxygen was blown through multipurpose side oxygen lance (103) with simultaneous addition of coke breeze for foamy slag practice. Arcing power was maintained to achieve the target tapping temperature of 1620-1640 deg C. 10 Once the target temperature and required tapping weight was achieved, arcing was finished and steel chemistry was analysed. The steel chemistry contains C = 0.050%, P = 0.015% and N = 30 pm and Si = 0.005%. From the above, it is clear that, the steel obtained by the method of the present disclosure 5 comprises composition of Nitrogen (N) being 30 ppm while the steel obtained by the conventional method had composition of Nitrogen (N) of about 50 ppm. Hence, the steel obtained by the method of the present disclosure possess better mechanical properties. EQUIVALENTS 10 With respect to the use of substantially any plural and/or singular terms herein, those having skill in the art can translate from the plural to the singular and/or from the singular to the plural as is appropriate to the context and/or application. The various singular/plural permutations may be expressly set forth herein for sake of clarity. 15 It will be understood by those within the art that, in general, terms used herein, and especially in the appended claims (e.g., bodies of the appended claims) are generally intended as "open" terms (e.g., the term "including" should be interpreted as "including but not limited to," the term "having" should be interpreted as "having at least," the term "includes" should be 20 interpreted as "includes but is not limited to," etc.). It will be further understood by those within the art that if a specific number of an introduced claim recitation is intended, such an intent will be explicitly recited in the claim, and in the absence of such recitation no such intent is present. For example, as an aid to understanding, the following appended claims may contain usage of the introductory phrases "at least one" and "one or more" to introduce 25 claim recitations. However, the use of such phrases should not be construed to imply that the introduction of a claim recitation by the indefinite articles "a" or "an" limits any particular claim containing such introduced claim recitation to inventions containing only one such recitation, even when the same claim includes the introductory phrases "one or more" or "at least one" and indefinite articles such as "a" or "an" (e.g., "a" and/or "an" should typically be 30 interpreted to mean "at least one" or "one or more"); the same holds true for the use of definite articles used to introduce claim recitations. In addition, even if a specific number of an introduced claim recitation is explicitly recited, those skilled in the art will recognize that such recitation should typically be interpreted to mean at least the recited number (e.g., the bare recitation of "two recitations," without other modifiers, typically means at least two 11 recitations, or two or more recitations). Furthermore, in those instances where a convention analogous to "at least one of A, B, and C, etc." is used, in general such a construction is intended in the sense one having skill in the art would understand the convention (e.g., "a system (100) having at least one of A, B, and C" would include but not be limited to systems 5 that have A alone, B alone, C alone, A and B together, A and C together, B and C together, and/or A, B, and C together, etc.). In those instances where a convention analogous to "at least one of A, B, or C, etc." is used, in general such a construction is intended in the sense one having skill in the art would understand the convention (e.g., "a system (100) having at least one of A, B, or C" would include but not be limited to systems that have A alone, B 10 alone, C alone, A and B together, A and C together, B and C together, and/or A, B, and C together, etc.). It will be further understood by those within the art that virtually any disjunctive word and/or phrase presenting two or more alternative terms, whether in the description, claims, or drawings, should be understood to contemplate the possibilities of including one of the terms, either of the terms, or both terms. For example, the phrase "A or 15 B" will be understood to include the possibilities of "A" or "B" or "A and B."

While various aspects and embodiments have been disclosed herein, other aspects and embodiments will be apparent to those skilled in the art. The various aspects and embodiments disclosed herein are for purposes of illustration and are not intended to be 20 limiting, with the true scope and spirit being indicated by the following claims. Referral Numerals: Referral Numerals Description 100 System 101 Support column 102 Pair of furnace shells 103 Oxygen blowing lance 104 Electrodes 201-205 Flow chart blocks 25 12 We Claim: 1. A method for controlling nitrogen content in a steel manufactured by CONverter ARCing (CONARC) steel making process, the method comprising: 5 addition of a bottom batch into a furnace shell (102); charging a hot metal into the furnace shell (102), wherein the hot metal comprises sulphur (S) composition in wt% ranging between 0.005%-0.01%; blowing a predetermined quantity of oxygen into the furnace shell (102) at a predetermined flow rate; 10 arcing in the furnace shell (102) for melting and to increase temperature to a tapping temperature; and tapping steel out of the furnace shell (102), wherein a tapped steel comprises composition of Nitrogen (N) in range of 30 ppm to 40 ppm. 15 2. The method as claimed in claim 1, wherein the bottom batch comprises calcined lime or calcined dolomite, direct reduced iron (DRI) and Cold briquetted iron (CBI). 3. The method as claimed in claim 1, wherein blowing of oxygen is performed by a water cooled oxygen lance (103). 20 4. The method as claimed in claim 1, wherein the predetermined flow rate of oxygen is 180-210 Nm3 /min. 5. The method as claimed in claim 1, wherein the predetermined quantity of oxygen ranges between 5000-6000 Nm3 25 . 6. The method as claimed in claim 1, comprising charging direct reduced iron (DRI) and Cold briquetted iron (CBI) into the furnace shell (102) as coolant during blowing of oxygen. 30 7. The method as claimed in claim 1, comprising charging direct reduced iron (DRI), Cold briquetted iron (CBI), calcined lime and calcined dolomite into the furnace shell (102), during arcing to increase charge mix. 13 8. The method as claimed in claim 1, wherein the tapping temperature ranges between 1620 °C -1640 °C. 9. A steel manufactured by a method as claimed in claim 1, the steel comprising: 5 an alloying composition (in wt.%) of: Carbon (C) of 0.050 wt.%, Phosphorous (P) of 0.015 wt.%, Nitrogen (N) ranging between 30 ppm to 40 ppm, Silicon (Si) of 0.005 wt.%, and 10 balance being substantially iron and incidental impurities.