"A Process For The Preparation Of Secondary Alcohols By Oxidation Of N Paraffins Using A Catalyst System"

National Research Development Corporation
Granted App No 1131/DEL/2002 Patent 248243 Chemical

Patent information

IP India · live record
Application number
1131/DEL/2002
Filing date
11 November 2002
Status
Granted
Legal status
Ceased
Publication number
10/2007
Publication type
INA
Invention field
Chemical
Patent number
248243
Grant date
29 June 2011
Next renewal due
11 November 2013Overdue

Abstract

This invention relates to a catalyst, useful for the preparation of secondary alcohols by oxidation of n-paraffins, which comprises a fatty acid salt of elements of Group II (a) of the periodic table of elements and a process for liquid phase oxidation of n-paraffins in presence of 10 to 1000 ppm of n-paraffin the said catalyst and 0.1 to 10 wt% of n-paraffin the boric acid/borate esters of fatty acids in which an individual n-paraffin mixture of n-paraffms are contacted with air or mixture of oxygen and inert gas such as nitrogen at space velocity of l-250h~1 and at temperature between 150-250°C and at pressure between atmosphere to 10 bar.

Applicants

1
India
NATIONAL RESEARCH DEVELOPMENT CORPORATION ANUSANDHAN VIKAS, 20-22, ZAMROODPUR COMMUNITY CENTRE, KAILASH COLONY EXTENSION, NEW DELHI-110 048, INDIA.

Inventors

4
India
A.K. BHATNAGARINDIAN INSTITUTE OF PETROLEUM,P.O.IIP, MPHKAMPUR, DEHRADUN-248005, INDIA.
India
A.K. GUPTAINDIAN INSTITUTE OF PETROLEUM,P.O.IIP, MPHKAMPUR, DEHRADUN-248005, INDIA.
India
S.C. JOSHIINDIAN INSTITUTE OF PETROLEUM,P.O.IIP, MPHKAMPUR, DEHRADUN-248005, INDIA.
India
H.B. GOYALINDIAN INSTITUTE OF PETROLEUM,P.O.IIP, MPHKAMPUR, DEHRADUN-248005, INDIA.

Claims

5
1 A process for the preparation of secondary alcohols in liquid phase by oxidation of n-paraffins with oxygen, air or oxygen containing inert gas which comprises:- (a) Contacting the n-paraffin with the catalyst as herein described the metal part of the catalyst being selected from the Group 11(a) of periodic table of elements, preferably Ca, Mg or Ba and organic legend with metal is a fatty ester group of C10-C20 carbon chain, preferably laurate, palmitate or stearate; wherein the said catalyst to n-paraffin ratio is 10 to 1000 ppm; (b) Contacting the resulting mixture with air or oxygen containing inert gas such as nitrogen and boric acid or borate ester at space velocity in the range 1-250 h-1, temperature in the range of 150-250°C, and pressure in the range of 0.01-10 bar for a period of 1-10h, wherein the boric acid or borate ester concentration is 0.1 to 10% wt of the n-paraffin; (c) Separating the secondary alcohol boric acid esters, unreacted n-paraffins unreacted boric acid by distillation; and (d) Recovering the secondary alcohols by hydrolysis of borate ester; and recycling the unreacted n-paraffins, and boric acid in the step (a) and (b) above.
2 The process as claimed in claim 1, wherein the catalyst to n- paraffin ratio ranges preferably between 10 to 500 ppm.
3 The process as claimed in claim 1, wherein the pressure is in the range of preferably 0.01-3 bar.
4 The process as claimed in claim 1, wherein the temperature is in the range of preferably 170-200°C.
5 The process for the preparation of secondary alcohols by oxidation of n-paraffins, wherein the catalyst system comprises catalyst which is a metal salt of a saturated fatty acid containing carbon atoms ranging between C10-C20 selected from palmitate or stearate.

Specification

Show full textCollapse

Background of the Invention This invention relates to a catalyst and a process for preparing secondary alcohols using the catalyst. The invention is particularly concerned with a catalyst comprising "of metal salt(s) of saturated fatty acids having carbon range from 10-20 which when used as catalyst in the oxidation of n-paraffins in presence of boric acid, dehydrated boric acid or boric acid esters, selectively, yields secondary alcohols. Fatty alcohols, having Ci2-C-i5 carbon chains and their derivatives are important commercial products as plasticizers, surfactants and in the production of polymers, monomers, lubricating oils. Viscosity improvers and pour point depressants greases etc. Fatty alcohol derivatives are used to a great extent in the premium house hold detergents for performance and environmental reasons. These surfactants are readily biodegradable and are finding increased use in low phosphate and nonphosphate detergertts. The alcohol provides the starting material for all types of surfactants e.g. non-ionics anianics, catiaric and zwitterianics of C12-Q find applications in consumer products e.g. Toothpaste, hair shampoos, carpet shampoos and light duty house hold detergent. Polyethoxylates alcohols sulphates and neutralized products gives anionic surfactants had wide applications as light duty detergent and heavy duty house hold liquid & granular detergent. Polyethoxylated alcohols have numerous industrial applications as wetting agents, dispersing agents and emulsifiers. It is well known in the literature that these fatty alcohols can be produced directly via oxidation of n-paraffins. Studies to prepare fatty alcohols via oxidation of n-paraffins. Studies to prepare fatty alcohols via oxidation of n-paraffins in presence of boric acid and arsenous acids, aluminium and chromic hydroxides and potassium permanganate are described in J. Soc. Chem. Ind. Jpn., 47, pp. 475-477, 1944; ibid- 46, pp. 765-7, 1943 and Ann. Chim. Appl., 39, pp. 311-20, 1949. In all the above investigations the alcohol formation is accompanied by the formation of large amount of by-products such as acids, esters and carboxyl compounds etc., resulting in a complex mixture of oxygenated compound; the isolation of alcohols from such complex mixture is very difficult. Bashkirov et.al. and Bashkirov and Kamzolkim (Proc. Acad. Sci. U.S.S.R. Chem. Tech. Sec., 1, pp 118-119, 1956 and World Pet. Congr. 4, pp. 175-183, 1959) described the process for oxidation of individual n-paraffins with nitrogen-oxygen mixture containing 3.0 to 4.5% oxygen at 165 -170°C mixture containing 3.0 to 4:5% oxygen in liquid phase at 165-170°C in presence of boric acid or -to produce secondary fatty alcohols with same number of carbon atoms and the same skeletal structure of the starting paraffin. The yield of alcohols was reported to be about 70% of the n-paraffins feedstock. Various boron derivatives e.g. tributoxy boroxine, tributoxy borane, boron trioxide with or without lithium oxide have also been reported to be used in the oxidation of nparaffin to alcohols. The yield of alcohols were however low in the range of 16-21% at 10-30% paraffin conversion. In US patent no. 3,238,238 (1966), use of oxidation catalysts such as Mg, Co or V napthenate, oleate or acetate with t-butylborate and an inert diluent oxidize aliphatic hydro-carbons to alcohols at 130-180°C. . Japanese patent no 6,27,267 (1987) describes a'process to prepare alcoholic waxes by liquid-phase oxidation of C2o-C6o paraffins waxes with oxygen in presence of 1.0:0.5 - 1.0 mol mixture of H3BO3 and B2O3; about 73% conversion to alcohols were reported. . A process for preparing secondary alcohols by oxidation of Ci0-C3o n-paraffins using finely divided orthoboric acid at 156-60°C has been claimed to given about 70% selectivity to alcohol formation. (Neth. Patent appl. 6, 50g857 (1966)). Use of promoters such as ammonia, amines, imides, amides, pyridine etc. were found to promote the oxidation of alkanes or cycloalkane with boric acid or dehydrate boric acid (French patent no - 1,501,429 (1967)). US patent no 4,970,346 (1990) disclose a process for the production of detergent range alcohols and ketones from Cio-Cia alkanes by reacting with a hydroperoxide in the presence of dicyano bis (1,10 = phenanthrolene) iron (II) catalyst. -3- The use of transition metal catalysts to prepare Cm-Cia alcohols have been described in US patent no's-4,978,800 (1990) and 4,978,799 (1990); the conversion to alcohols obtained were low (~ 2% wt) even at longer reaction time of 20 h. The oxidation of alkanes in presence of boric acid or esters to produce alcohols was claimed to be accelerated by use of 50-100 ppm transition metal as a 3dcarboxylate. (Brit. Patent no -1,035,624 (1966)). Various oxidation catalysts were reported in literature including Mn-Naphthenate MnOa, KMnO4, t-Butyl per oxide, Co-strearate, TiCU, etc. to increase the yield of Borate ester. Amine & NHa were used to reduce the deactivation effect of aromatics. Use of additives such as boron trioxide, tributyl oxyboroxine, oxybis (di-n-butoxy borane) and t-butyl hydroperoxide is known to increase, the formation of alcohols but ' only marginally. In the hitherto known processes, generally the yield of alcohols and conversion of n-paraffms perpass is low and range between 16-21% and 10-30% respectively. The selectivity of alcohols and ketones combined together.range between 80-90% based on paraffin. Further in these processes there is always a possibility of coagulation of boric acid or boric acid esters due to their poor solubility and density difference between boric acid and hydrocarbon phase. This leads to poor activity of boric acid and lower yield of alcohols. The main object of the present invention is to provide a catalyst that provide an improved process for the oxidation of paraffins. It is an object of the present invention to provide a process in which the use of the said catalyst increases the yield of secondary alcohols in the oxidation of paraffins. It is yet another object of the present invention to provide catalyst that increases the rate of initiation of peroxides in the free radical oxidation of paraffins and thereby increasing the formation and selectivity of secondary alcohols. STATEMENT OF INVENTION According to this invention there is provided a process for the preparation of secondary alcohols in liquid phase by oxidation of n-paraffins with oxygen, air or oxygen containing inert gas which comprises Contacting the n-paraffin with the catalyst as herein described the metal part of the catalyst being selected from the Group 11(a) of periodic table of elements, preferably Ca, Mg or Ba and organic legend with metal is a fatty ester group of C10-C20 carbon chain, preferably laurate, palmitate or stearate; wherein the said catalyst to n-paraffin ratio is 10 to 1000 ppm; Contacting the resulting mixture with air or oxygen containing inert gas such as nitrogen and boric acid or borate ester at space velocity in the range 1-250 h-1, temperature in the range of 150-250°C, and pressure in the range of 0.01-10 bar for a period of 1-1 Oh, wherein the boric acid or borate ester concentration is 0.1 to 10% wt of the n-paraffin; Separating the secondary alcohol boric acid esters, unreacted n-paraffins unreacted boric acid by distillation; and Recovering the secondary alcohols by hydrolysis of borate ester; and recycling the unreacted n-paraffins, and boric acid in the step (a) and (b) above. SUMMERY OF THE INVENTION In accordance with the present invention, it has been found that catalysts comprising of metal salts of long chain fatty acids exhibit very high activity and selectivity, when used to produce secondary alcohols via oxidation of n-paraffins in presence of boric acid/boric acid ester. The metal part of the catalyst of the catalyst is a metal selected from Group-II (a) of her Periodic Table of Elements. The fatty acid part is selected from C10-C20 saturated fatty acids. The catalytic salts described in the present invention can be prepared by conventional technique used in the preparation of metal salts of fatty acids. The inventors of the present invention conducted repeated research regarding the use of Group-11(a) metal salts of fatty acids as catalyst to enhance rate of oxidation of n-paraffin and selectivity to secondary alcohols in presence of boric acid/fatty acid borate esters and found that the fatty acid salts of Mg, Ca or Ba are particularly useful in enhancing the rate of initiation step in oxidation of n-paraffins, using molecular oxygen/air or Nitrogen oxygen mixture, and selectivity to secondary alcohols. The present further relates to the application of Group-II (a) metal salts of fatty acids and provides a process to oxidize n-paraffins with 02/air/nitrogen and oxygen mixture in presence of boric acid under moderate operating conditions to selectively produce secondary alcohols. The oxidation reaction was carried out in cylindrical reactor having a sintered disc at the bottom to bubble the N2 + 02 mixture. The reactor was connected to a reflex condenser through Dean and Stark receiver to remove water. The paraffin feed along with the catalyst is taken in the reactor while N2 + 02 mixture of known concentration is bubbled through the paraffin at a required rate, space velocity ranging between 1-250 h-1. The concentration of the catalyst used is in the range of 10 to 1000 ppm of n-paraffins. The contents of the reactor is heated to the desired temperature and then boric acid 0.1 to 10 wt% of n-paraffin is added to it; the reaction is continued and the water form the reactor is removed with the help of Dean and stark separator. After the reaction is over product is cooled and taken out in a RB flask. Unreacted paraffin is removed under reduced pressure to the extent -fpossible. The extent & yield of the alcohols were .monitored in terms of the yield of Borate ester. The borate ester left as residue is hydrolysed with equal quantity of water at reflux temperature. The aqueous layer is evaporated to recover boric acid. The organic portion is digested with alkali to remove organic acid which can be recovered by neutralization of aqueous portion. The organic portion is again distilled to recover the secondary alcohols. It will be apparent from the foregoing that the present invention provides a catalyst which is active and selective for producing secondary alcohols via oxidation of n-paraffins. Moreover the catalyst of the present invention which comprises a salt of Group-ll(a) metal and a long chain fatty acid having C-i2-C2o carbon atoms preferably laurate, palmitate or stearate is unexpectedly active and selective for oxidation of nparaffins to produce secondary alcohols. It was found that the oxidation reaction of n-paraffins jrv presence of the catalyst of the present invention follows the free radical mechanism comprising of initiation, propagation and termination steps. The overall rate of reaction is controlled by transfer of oxygen through the gas-liquid interface. The catalyst of the present invention enhances the gas-liquid interfacial area and in turn increases the rate of initiation i.e. formation of peroxides. The increased rate of peroxide formation further increases the formation of borate esters which is an equilibrium reaction. The invention will be described in more details with reference to the following ' examples. These examples, however, are not to be construed to limit the scope of the invention. Although the invention has been described in conjunction with examples and by reference to the embodiments thereof, it is evident that many alternatives, modifications, and variations will be apparent to those skilled in the art in light of the foregoing description, accordingly it is intended in the invention to embrace these and all such alternatives, variations, and modifications as may fail within the spirit and scope of the appended claimsExample-1 100 g of the n-paraffins mixture was taken in a cylindrical glass reactor having a sintered disc at the bottom to bubble the oxygen nitrogen mixture' (oxygen content 4,5%). The oxygen nitrogen mixture was bubbled at the rate of 40 litre p«r hour and the temperature from room temperature was increased to 180°C in 60 minutes. Peroxide value of the paraffin mixture after 15 minutes was found to be 42.3 meq/kg. 3 g of boric acid in 25 ml of water was added to the system in 45 minutes. A second lot of 3g boric acid in 25 ml water was again added in 45 minutes. The reaction was continued for 180 minutes. The water along with same paraffin was collected in Dean and Stark receiver which was removed from time to time while paraffin was returned to the reactor. After the reaction was over the unreacted paraffin was removed by distillation under reduced pressure and residue was hydrolysed with 'water to decompose the borate ester of secondary alcohol. The organic layer thus obtained was refluxed with sodium hydroxide solution. After 15 minutes the organic layer was washed with water and distilled to obtain secondary alcohol. The yield of alcohol thus obtained was 18.9%. Example-2 100 g of n paraffin mixture of Cio-Cu along with 0.041 g of Magnesium laurate was taken in a cylindrical glass reactor as described in example-1. The mixture was treated with oxygen; nitrogen mixture at a rate of 40 liter per/ hour and temperature was slowly increased to 180°C in 60 min. The peroxide value of the paraffin mixture after attaining the reaction temperature was found to be 127.8 meq./kg. 3 g of boric acid in 25 ml water was added in 30 minutes. A second lot of 3 g boric acid in 25 ml water was again added in 30 minutes and reaction was continued for 240 minutes. After work up as described in example-1 the yield secondary of alcohols was found to be 32.7%. Example-3 The experiment was carried out as described in exaple-2 except that 0.0435 < barium laurate was used in this experiment. The peroxide value observed, after 1: minutes of attaining the temperature of 180°C was 96.85 meq/kg. The yield c secondary alcohols obtained was 27.65%. Example-4 The experiment was as described in example-3 except that 0.0422 g of calcium laurate was in place of barium laurate. After 15 minutes of attaining the reaction temperature (180°C) the peroxide value of the reaction mixture was found to be 195.35 meq/kg. The yield of alcohols was found to be 32.78%.'

]

WE CLAIM: 1. A process for the preparation of secondary alcohols in liquid phase by oxidation of n-paraffins with oxygen, air or oxygen containing inert gas which comprises:- (a) Contacting the n-paraffin with the catalyst as herein described the metal part of the catalyst being selected from the Group 11(a) of periodic table of elements, preferably Ca, Mg or Ba and organic legend with metal is a fatty ester group of C10-C20 carbon chain, preferably laurate, palmitate or stearate; wherein the said catalyst to n-paraffin ratio is 10 to 1000 ppm; (b) Contacting the resulting mixture with air or oxygen containing inert gas such as nitrogen and boric acid or borate ester at space velocity in the range 1-250 h-1, temperature in the range of 150-250°C, and pressure in the range of 0.01-10 bar for a period of 1-10h, wherein the boric acid or borate ester concentration is 0.1 to 10% wt of the n-paraffin; (c) Separating the secondary alcohol boric acid esters, unreacted n-paraffins unreacted boric acid by distillation; and (d) Recovering the secondary alcohols by hydrolysis of borate ester; and recycling the unreacted n-paraffins, and boric acid in the step (a) and (b) above. 2. The process as claimed in claim 1, wherein the catalyst to n-paraffin ratio ranges preferably between 10 to 500 ppm. 3. The process as claimed in claim 1, wherein the pressure is in the range of preferably 0.01-3 bar. 4. The process as claimed in claim 1, wherein the temperature is in the range of preferably 170-200°C. 5. The process for the preparation of secondary alcohols by oxidation of n-paraffins, wherein the catalyst system comprises catalyst which is a metal salt of a saturated fatty acid containing carbon atoms ranging between C10-C20 selected from palmitate or stearate.

Documents

Sign in to open
Application documents
1 1131-DEL-2002-GPA-(08-02-2010).pdf 08 Feb 2010
2 1131-DEL-2002-Form-5-(08-02-2010).pdf 08 Feb 2010
3 1131-DEL-2002-Form-3-(08-02-2010).pdf 08 Feb 2010
4 1131-DEL-2002-Form-1-(08-02-2010).pdf 08 Feb 2010
5 1131-DEL-2002-Description (Complete)-(08-02-2010).pdf 08 Feb 2010
6 1131-DEL-2002-Correspondence-Others (08-02-2010).pdf 08 Feb 2010
7 1131-DEL-2002-Claims-(08-02-2010).pdf 08 Feb 2010
8 1131-DEL-2002-Abstract-(08-02-2010).pdf 08 Feb 2010
9 1131-del-2002-form-2 (24-06-2011).pdf 24 Jun 2011
10 1131-del-2002-Form-1 (24-06-2011).pdf 24 Jun 2011
11 1131-del-2002-Correspondence-others (24-06-2011).pdf 24 Jun 2011
12 1131-DEL-2002-Correspondence Others-(24-06-2011).pdf 24 Jun 2011
13 1131-del-2002-Claims (24-06-2011).pdf 24 Jun 2011
14 1131-del-2002-Amended Of Specification-(24-06-2011).pdf 24 Jun 2011
15 1131-DEL-2002-Abstract-(24-06-2011).pdf 24 Jun 2011
16 1131-del-2002-Abstract (24-06-2011).pdf 24 Jun 2011
17 1131-del-2002-gpa.pdf 21 Aug 2011
18 1131-del-2002-form-3.pdf 21 Aug 2011
19 1131-del-2002-form-2.pdf 21 Aug 2011
20 1131-del-2002-form-18.pdf 21 Aug 2011
21 1131-del-2002-form-1.pdf 21 Aug 2011
22 1131-del-2002-description (complete).pdf 21 Aug 2011
23 1131-del-2002-correspondence-po.pdf 21 Aug 2011
24 1131-del-2002-correspondence-others.pdf 21 Aug 2011
25 1131-del-2002-claims.pdf 21 Aug 2011
26 1131-del-2002-abstract.pdf 21 Aug 2011
27 1131-DEL-2002_EXAMREPORT.pdf 30 Jun 2016

ERegister / renewals

Ceased
3rd Renewed 12 Jul 2011 Period 11 Nov 2004 – 11 Nov 2005 · CBR 6324 · Certificate 7114 ₹2,000
4th Renewed 12 Jul 2011 Period 11 Nov 2005 – 11 Nov 2006 · CBR 6324 · Certificate 7114 ₹2,000
5th Renewed 12 Jul 2011 Period 11 Nov 2006 – 11 Nov 2007 · CBR 6324 · Certificate 7114 ₹2,000
6th Renewed 12 Jul 2011 Period 11 Nov 2007 – 11 Nov 2008 · CBR 6324 · Certificate 7114 ₹2,000
7th Renewed 12 Jul 2011 Period 11 Nov 2008 – 11 Nov 2009 · CBR 6324 · Certificate 7114 ₹6,000
8th Renewed 12 Jul 2011 Period 11 Nov 2009 – 11 Nov 2010 · CBR 6324 · Certificate 7114 ₹6,000
9th Renewed 12 Jul 2011 Period 11 Nov 2010 – 11 Nov 2011 · CBR 6324 · Certificate 7114 ₹6,000
10th Renewed 12 Jul 2011 Period 11 Nov 2011 – 11 Nov 2012 · CBR 6324 · Certificate 7114 ₹6,000
11th Renewed 19 Oct 2012 Period 11 Nov 2012 – 11 Nov 2013 · CBR 10434 · Certificate 10093 ₹12,000