A Process For The Synthesis Of Spheroidal Magnesium Alkoxide

Reliance Industries Limited
Granted App No 916/MUM/2008 Patent 251446 Chemical

Patent information

IP India · live record
Application number
916/MUM/2008
Filing date
25 April 2008
Status
Granted
Legal status
Inforce
Publication number
45/2009
Publication type
INA
Invention field
Chemical
Patent number
251446
Grant date
16 March 2012
Next renewal due
25 April 2027

Abstract

The invention relates to a process for the synthesis of spheroidal magnesium alkoxide having improved mechanical strength and narrow particle size distribution, the process comprising reacting magnesium metal, in the presence of iodine, with a mixture of alcohols by step-wise heating first in the range of 40°C to 65°C for a period of 2 hours and then in the range of 65°C to 80°C for a period of 1 hour, further by maintaining reaction temperature at 80°C for a period of 6 - 10 hours, the vapours of the mixture produced during the reaction being condensed in an overhead condenser, hydrogen gas produced during the reaction being vented off and the mixture of alcohols left after the reaction being filtered and reused. The invention also relates to spheroidal magnesium alkoxide particles synthesized by the method, to the Ziegler natta procatalyst synthesized by using the alkoxide and to the polymer resin synthesised using the procatalyst.

Applicants

1
India
RELIANCE INDUSTRIES LIMITED 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT,

Inventors

9
India
GUPTA VIRENDRAKUMARRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
SINGH SAURABHRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
MAKWANA UMESHRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
JOSEPH JOMICHANRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
SINGALA KAMLESRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
RAJESH SMITHARELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
PATEL VALLABHBHAIRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
YADAV MUKESKUMARRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,
India
SINGH GURMEETRELIANCE INDUSTRIES LIMITED, 5TH FLOOR, MAKER CHAMBER IV, NARIMAN POINT, MUMBAI 400021,

Specification

Show full textCollapse

FORM 2 THE PATENTS ACT, 1970 (39 of 1970) As amended by the Patents (Amendment) Act, 2005 & The Patents Rules, 2003 As amended by the Patents (Amendment) Rules, 2005 COMPLETE SPECIFICATION (See section 10 and rule 13) 1. TITLE OF THE INVENTION Spheroidal particles for olefin polymerization catalyst APPLICANTS Name : Reliance Industries Limited Nationality : An Indian company Address : 5th Floor, Maker Chamber IV, Nariman Point, Mumbai 400 021, Maharashtra, India 2. INVENTORS Names : Gupta, Virendrakumar; Singh, Saurabh; Makwana Umesh; Joseph, Jomichan; Singala, Kamlesh; Rajesh, Smitha; Patel, Vallabhbhai; Yadav, Mukeshkumar; Singh, Gurmeet; Nationality : All Indian Nationals Address : All of Reliance Industries Limited, 5 Floor, Maker Chamber IV, Nariman Point, Mumbai 400 021, Maharashtra, India 3. PREAMBLE TO THE DESCRIPTION The following specification particularly describes the nature of this invention and the manner in which it is to be performed:

Field of Invention The invention relates to spheroidal magnesium alkoxide particles having improved mechanical strength and narrow particle size distribution. The invention also relates to a method for synthesis of the alkoxide , to the Ziegler Natta procatalyst synthesized by using the alkoxide and to the polymer resin synthesised using the procatalyst. Background of Invention Resin particles having regular shape and narrow particle size distribution are desirable for good flowability during resin extrusion. They are also essential to produce regular shaped copolymer products with uniform rubber dispersion. Shape regularity and size distribution of polymer resin are usually related to the shape and size of the catalyst particles as well as of the solid reactants from which the catalyst particles are synthesized. Solid magnesium ethoxide is used as the reactant for the synthesis of Ziegler Natta catalysts used for olefin polymerization. WO 2005/044873 discloses a method for synthesizing spherical magnesium alkoxide particles by reacting magnesium with an alcohol mixture at a temperature below the boiling point of the mixture. The spherical magnesium alkoxide particles synthesized by the method are rather frangible and do not retain their morphology or particle size during the synthesis of Ziegler Natta procatalyst, especially when the procatalyst synthesis is carried out on a large scale. Further, the particle size distribution of the alkoxide particles synthesized by the above mentioned method need improvement.

Detailed Description Accordingly, the invention provides a process for synthesis of spheroidal magnesium alkoxide particles having improved mechanical strength and narrow particle size distribution. In one embodiment, the invention provides a process for the synthesis of spheroidal magnesium alkoxide having improved mechanical strength and narrow particle size distribution, the process comprising reacting magnesium metal, in the presence of iodine, with a mixture of alcohols by step-wise heating first in the range of 40°C to 65°C for a period of 2 hours and then in the range of 65°C to 80°C for a period of 1 hour, further by maintaining reaction temperature at 80°C for a period of 6 to 10 hours, the vapours of the mixture produced during the reaction being condensed in an overhead condenser, hydrogen gas produced during the reaction being vented off and the mixture of alcohols left after the reaction being filtered and reused. In another embodiment, the invention provides a process for the synthesis of spheroidal magnesium alkoxide having improved mechanical strength and narrow particle size distribution, the process comprising reacting magnesium metal, in the presence of iodine, with a mixture of alcohols by step-wise heating first in the range of 40°C to 65°C for a period of 2 hours and then in the range of 65°C to 80°C for a period of 1 hour, further by maintaining reaction temperature at 80°C for a period of 6 to 10 hours, the vapours of the mixture produced during the reaction being condensed in an overhead condenser, hydrogen gas produced during the reaction being vented off and the mixture of alcohols

left after the reaction being filtered and reused, the mixture of alcohols being selected from the group consisting of methanol, ethanol, propanol, isopropanol, butanol and isobutanol. In another embodiment, the invention provides a process for the synthesis of spheroidal magnesium alkoxide having improved mechanical strength and narrow particle size distribution, the process comprising reacting magnesium metal, in the presence of iodine, with a mixture of alcohols by step-wise heating first in the range of 40°C to 65°C for a period of 2 hours and then in the range of 65°C to 80°C for a period of 1 hour, further by maintaining reaction temperature at 80°C for a period of 6 to 10 hours, the vapours of the mixture produced during the reaction being condensed in an overhead condenser, hydrogen gas produced during the reaction being vented off and the mixture of alcohols left after the reaction being filtered and reused, ratio of magnesium metal to the mixture of alcohols being in the range of 1: 2 to 1: 20 In another embodiment, the invention provides spheroidal magnesium alkoxide particles, the particles comprising at least two different alkoxy groups, one alkoxy group being present in less than 40 percentage by weight and another alkoxy group being present in greater than 40 percentage by weight of the particles. In another embodiment, the invention provides spheroidal magnesium alkoxide particles having circularity in the range of 0.5 to 1.0, mean particle size in the range of 25 to 65

microns, bulk density in the range of 0.45 to 0.65 g/cc, span less than 1.5, surface area in the range of 1 to 20 m2/g and crushing strength of at least 20 kg. In another embodiment, the invention provides spheroidal magnesium alkoxide particles exhibiting a diffraction pattern on irradiation with a Cu Ka radiation having a wavelength of 1.5406 A0, the diffraction pattern comprising peaks at 2 0 values of around 9.8, 10.2, 10.4 and 11.9. In another embodiment, the invention provides a method for synthesis of Ziegler Nata procatalyst, the method comprising reacting spheroidal magnesium alkoxide particles with TiCl4 and chlorobenzene, the method yielding a side product having the formula TiClx(OR1)y(OR2)z where x, y, z is an integer from 0 to 4 and R1, R2 is an alkyl or an aryl group, the side product on treatment with a carboxylic acid chloride generating in situ internal donors for the procatalyst. In another embodiment, the invention provides spheroidal Ziegler Natta procatalyst having a particle size in the range of 25 to 65 microns and comprising internal donor(s) generated in situ In another embodiment, the invention provides spheroidal Ziegler Natta procatalyst comprising internal donor(s) selected from the group consisting of methyl benzoate, ethyl benzoate, n-propyl benzoate, i-propyl benzoate, n-butyl benzoate, i-butyl benzoate,

dimethyl phthalate, diethyl phthalate, dipropyl phthalate, di-isopropyl phthalate, di-butyl phthalate and di-isobutyl phthalate In a further embodiment, the invention provides a method for polymerization of olefin, the method comprising contacting the olefin with a catalyst system comprising spheroidal Ziegler Natta procatalyst, triethyl alumunium cocatalyst optionally along with a selectivity control agent. In a still further embodiment of the invention, there is provided spheroidal polyolefin particles synthesised by the method comprising contacting the olefin with a catalyst system comprising spheroidal Ziegler Natta procatalyst, triethyl alumunium cocatalyst optionally along with a selectivity control agent. The invention provides a process for synthesis of spheroidal magnesium alkoxides having improved mechanical strength and narrow particle size distribution by reacting magnesium metal with a mixture of alcohols. The magnesium metal can be in the form of powder, granules or ribbon. The ratio of magnesium to the mixture of alcohols can be in the range of 1:2 to 1:20. The reaction is usually carried out at a temperature in the range of20°Ctol00°Candat a pressure of 0.1 to 5.0 atm. Reaction temperature is increased in a step wise manner to have improved kinetic control. The vapours of the alcohol mixture was recovered by condensing in the overhead condenser. The alcohol mixture left after the reaction was filtered and the filtrate was reused for the synthesis. The hydrogen gas produced during the synthesis was vented off. The reaction is carried out in the presence

of an initiator such as iodine. Any halogen or halogen containing compound other than iodine can as well be used as the initiator. The mixture of alcohols used for the reaction is selected from the group consisting of methanol, ethanol, propanol, isopropanol, butanol and isobutanol. Other aliphatic/ aromatic alcohols can as well be used for the reaction. Preferably, the mixture contain two alcohols, one of which is ethanol. One of the alcohols in the mixture is used in excess to work as the reaction solvent. Further, the reaction is carried out under inert atmosphere. The inert atmosphere is created in situ by hydrogen gas which is produced during the reaction. The spheroidal magnesium alkoxide particles of the invention comprise at least two different alkoxy groups, one alkoxy group being present in less than 40 percentage by weight and another alkoxy group being present in greater than 40 percentage by total weight of the particles. Preferably the alkoxy group that is present in greater than 40 percentage by weight of the total alkoxy content is an ethoxy group. The alkoxide particles of the invention have low surface area, typically in the range of 1 to 20 m /g. Apart from its utility in the synthesis of spheroidal Ziegler Natta procatalyst, the spheroidal alkoxide particles of the invention can be used for other applications as well. The spheroidal alkoxide particles of the invention can be used for coating inorganic support materials such as silica or zeolites. The spheroidal magnesium alkoxide particles of the invention are used for the synthesis of spheroidal Ziegler Natta procatalyst. The alkoxide particles can be optionally pretreated with titanium tetrachloride, before the procatalyst synthesis. The pretreatment

is usually carried out by a 2-5 wt% solution of titanium tetrachloride in aromatic or aliphatic solvent. The procatalyst synthesis involves reaction of the magnesium alkoxide particles with TiCU and chlorobenzene wherein TiClx(OR1)y(OR2)z, where x, y, z is an integer from 0 to 4 and R , R is an alkyl or aryl group, is formed as a side product along with the procatalyst, during the synthesis. The side product is treated with a carboxylic acid chloride and the treatment results in the generation of internal donors. The preferred carboxylic acid chloride is benzoyl chloride. The quantity of in situ generated internal donors and consequently the composition of the procatalyst can be varied by varying the composition of magnesium alkoxide and amount of carboxylic acid chloride used for the treatment. The internal donors are used up during the synthesis of the procatalyst. The spheroidal procatalyst can be a diester based catalyst or a monoester based catalyst. Depending upon the specific requirements, catalysts based on other kind of internal donors can be prepared. Further, the spheroidal alkoxide particles of the invention can be used for the synthesis of spheroidal procatalyst on a large scale. The spheroidal procatalyst of the invention is used for the synthesis of spheroidal/ regular shaped polyolefin resin having narrow particle size distribution and improved particle size. The molecular weight distribution of the polyolefin can be varied by varying the composition of internal donor in the catalyst. The invention provides an economical method for synthesis of spheroidal magnesium alkoxide particles by recovering and reusing the mixture of alcohols used for the synthesis. The mixture of solvents is recovered through the vent condenser during the drying of the cake obtained after the reaction. Filtrate collected during slurry filtration is

also directly reused. Further, the invention provides spheroidal magnesium alkoxide particles having regular shape, with narrow particle size distribution, high bulk density, high mechanical strength and crystallinity. The magnesium alkoxide particles, the Ziegler natta procatalyst and the polyolefin resin in the following examples have been characterised by various methods. The alkoxy content of the alkoxide particles are measured by gas chromatography of the solution made by hydrolyzing magnesium alkoxide in dilute mineral acid. The mean particle size and span is obtained by particle size analyzer using laser and optical diffraction method on CILAS 1180 particle size analyzer. Span is calculated by ratio of (D90-D10)D50 where if Dn = X microns then it signifies that n% of the total particle population is below X microns. Bulk density is measured by measuring the tapped volume and weight of certain quantity of powder and by dividing weight of the powder by the tapped volume. The circularity is measured from the analysis of scanning electron microscope image using an image analysis software. Circularity of a particle is = (area of 2 dimensional particle image)/(area of circle having same parameter as the particle). X-ray powder patterns were recorded using Bruker Advance D8 diffractometer. Morphology was explored with FEI Inspect Scanning Electron Microscope. Crushing strength was determined by applying a force increasing with constant rate to fixed volume of solid powder mass in a cylindrical vessel and determining the minimum force required for compressing the mass by 1 mm on veritical axis of force application. Donor content is determined using high pressure liquid chromatography of the catalyst solution in methanol. Polymer bulk density is

calculated by measuring tapped volume and weight of fixed polymer resin quantity and then dividing weight by volume. The invention is further illustrated by way of the following examples EXAMPLES Example 1: Synthesis of spheroidal magnesium alkoxide particles with stepwise heating of reactants Magnesium powder (5.5 kg) was added to mixture of ethanol and methanol (125 L) in presence of initiator iodine (150 gm) at 40 °C with continued stirring. Making use of reaction exothermicity and external temperature control, reaction was conducted in a step-wise manner, heating first in the range to 40°C to 65°C for a period of 2 hrs and then in the range of 65°C to 80°C for a period of 1 hour, further by maintaining reaction temperature at 80°C for a period of 7 hours. The vapours of the mixture produced during the reaction was condensed in an overhead condenser. The hydrogen gas produced during the reaction was vented off and the mixture of alcohols left after the reaction was removed by filtration. The filtrate was reused for the synthesis. A wet cake was obtained after removal of the filtrate. The wet cake was dried to obtain 25 kg of white free flowing spheroidal particles having a bulk density of 0.50 - 0.60 g/cc and surface area of l0m 7g.

Example 2: Synthesis of magnesium alkoxide particles without stepwise heating of reactants Magnesium powder (5.5 kg) was added to mixture of alcohol having 65 Litres ethanol, 4 Litres Methanol and 2 litres isopropanol. 420 g of iodine was added in the form of solution in ethanol. Reaction mixture was heated to 50 °C and reaction was carried on till hydrogen evolution was stopped. The product was filtered and dried. Example 3: Synthesis of Ziegler natta procatalyst using magnesium alkoxide of example 1 The magnesium alkoxide (50 kg) from example 1 was treated with a equal volume mixture of 1150 liters TiCU and chlorobenzene in three step treatment at 100 °C. Internal donor Ethyl Benzoate is added in first step. Benzoyl Chloride is added in the last step. After three stage treatment solid procatalyst is filtered and given four washes with 1000 litres isopentane each and then it is dried at 50 °C under stream of nitrogen. 55 kg of yellow colored procatalyst was obtained. Example 4: Synthesis of Ziegler natta procatalyst using magnesium alkoxide of example 2 The magnesium alkoxide precursor (50 kg)) from example 2 was treated with a equal volume mixture of 1150 liters TiCl4 and Chlorobenzene in a three stage treatment at 100 °C. Internal donor ethyl benzoate is added in first step. Benzoyl Chloride is added in the last step. After three stage treatment solid procatalyst is filtered and given four washes

with 1000 litres isopentane each then dried at 50 °C under stream of nitrogen. 53 kg of yellow colored procatalyst was obtained. Example 5: Polymerisation of propylene using procatalyst of example 3 Solid procatalyst (0.08 g) of example 3 was mixed with triethyl alumunium cocatalyst (1.2 g) and paraethoxy ethylbenzoate (0.05 g). The catalysts were mixed in such proportions that the alumunium : titanium ratio is maintained at 250:1. The mole ratio of selectivity control agent to titanium was kept at 50:1. The catalyst was employed to polymerize propylene in slurry phase with hexane as the diluent under a constant propylene pressure of 5 kg for 1 hr at 70 °C, followed by addition of 50 mmol of hydrogen to terminate the polymerization Example 6: Polymerisation of propylene using procatalyst of example 4 Solid procatalyst (0.08 g) of example 4 was mixed with triethyl alumunium cocatalyst (1.2 g) and paraethoxy ethylbenzoate (0.05 g). The catalysts were mixed in such proportions that the alumunium : titanium ratio was maintained as 250:1. The mole ratio of selectivity control agent to titanium was kept at 50:1. The catalyst was employed to polymerize propylene in slurry phase with hexane as the diluent under a constant propylene pressure of 5 kg for 1 hr at 70 °C, followed by addition of 50 mmol of hydrogen to terminate the polymerization.

Table 1: Comparative analysis of spheroidal magnesium alkoxide particles of example 1 and example 2

Magnesium alkoxide prepared by Methoxycontent(wt%) Ethoxy content (wt%) i-propoxycontent(wt%) Mean Particle size (microns) Span BulkDensity(g/ml) Crushingstrength(kg) circularity Example 1 18.0 60.0 nil 34.0 0.82 0.59 30.2 0.72 Example 2 7.0 70.0 1.5 26.0 0.95 0.48 16.8 0.65 Table 2: Comparative analysis of Zieglar Natta procatalyst synthesized by using the alkoxide particles of example 1 and example 2

Procatalyst prepared by Meanparticlesize Span Circularity Example 3 34 1.14 0.73 Example 4 13 2.87 NA Table 3: Comparative analysis of polymer resins synthesized by using the ziegler natta procatalysts of example 3 and example 4

Polymer resin prepared by Meanparticlesize Span Bulk density Circularity Example 5 722 1.14 0.38 0.71 Example 6 320 2.79 0.32 NA Table 1 provides a comparative analysis of the magnesium alkoxide particles of the invention (prepared as in example 1) and of the alkoxide particles prepared as in example 2. The magnesium alkoxide particles of the invention had more circularity as compared to the magnesium alkoxide particles of example 2. Further, the crushing strength, particle size and bulk density of the particles of the invention are considerably higher than those

prepared by example 2. The alkoxide particles of the invention possess narrow particle size distribution as evidenced by their low span values. Table 2 compares the properties of the Ziegler natta procatalyst prepared (as in examples 3 and 4 respectively) by using the alkoxide particles of example 1 and example 2. It can be seen that there is shape replication during the procatalyst synthesis of example 3 and circularity as observed in the alkoxide particles is almost retained in the procatalyst. Further, particle size values of the procatalyst of the invention suggests negligible attrition for the particles of the invention. Further, the procatalyst prepared by the alkoxide particles of the invention has narrow particle size distribution as evidenced by their low values of span. Table 3 compares the properties of the polymer resin prepared (as in examples 5 and 6) by using the procatalyst of example 5 and example 6. The resin particles prepared by example 5 have high particle size, narrow particle size distribution as well as high bulk density and circularity as compared to the resin particles prepared by example 6. The morphology of the alkoxide particles, procatalyst particles and the resin particles of the invention is compared in the respective SEM images of the particles. Figure 1, Figure 3 and Figure 5 of the accompanying drawings present the SEM images of the alkoxide particles, of the procatalyst particles and of the resin particles of the invention. Figure 2, Figure 4 and Figure 6 of the accompanying drawings present the SEM images of the alkoxide particles, of the procatalyst particles and of the resin particles prepared by

example 2, example 4 and example 6 respectively. It can be clearly observed that the particles of the invention have regular spheroidal morphology which is retained during the procatalyst synthesis as well as during the resin synthesis. The invention, thus provides crystalline magnesium alkoxide particles having improved mechanical strength and narrow particle size distribution. Further, the alkoxide particles of the invention retains its morphology and particle size during subsequent procatalyst synthesis on a large scale. Furthermore, the retention of particle morphology is observed during the synthesis of the polymer resin. Therefore the magnesium alkoxide particles of the invention are suitable as precursors for the synthesis of regular shaped procatalyst and polymer resin. The invention also provides an economical, safe and environmentally friendly method for the synthesis of magnesium alkoxide particles by providing means for recovery and reuse of alcohol vapours during the alkoxide synthesis as well as by providing means for venting off the hydrogen gas produced during the synthesis. The above description is illustrative only and is not limiting. The present invention is defined by the claims that follow and their full range of equivalents.

We Claim 1. A process for the synthesis of spheroidal magnesium alkoxide having improved mechanical strength and narrow particle size distribution, the process comprising reacting magnesium metal, in the presence of iodine, with a mixture of alcohols by step-wise heating first in the range of 40°C to 65°C for a period of 2 hours and then in the range of 65°C to 80°C for a period of 1 hour, further by maintaining reaction temperature at 80°C for a period of 6 to 10 hours, the vapours of the mixture produced during the reaction being condensed in an overhead condenser, hydrogen gas produced during the reaction being vented off and the mixture of alcohols left after the reaction being filtered and reused. 2. The process as claimed in claim 1 wherein the mixture of alcohols is selected from the group consisting of methanol, ethanol, propanol, isopropanol, butanol and isobutanol. 3. The process as claimed in claim 1 wherein the ratio of magnesium to the mixture of alcohols is in the range of 1: 2 to 1: 20 4. Spheroidal magnesium alkoxide particles synthesized by the process as claimed in any one of the above claims, the particles comprising at least two different alkoxy groups, one alkoxy group being present in less than 40 percentage by weight of the particles and another alkoxy group being present in greater than 40 percentage by weight of the particles.

5. Spheroidal magnesium alkoxide particles having circularity in the range of 0.5 to 1.0, mean particle size in the range of 25 microns to 65 microns, bulk density in the range of 0.45g /cc to 0.65 g/cc, surface area in the range of 1 to 20 m /g and crushing strength of at least 20 kg. 6. Spheroidal magnesium alkoxide particles exhibiting a diffraction pattern on irradiation with a Cu Ka radiation having a wavelength of 1.5406 A0, the diffraction pattern comprising peaks at 2 0 values of around 9.8, 10.2, 10.4 and 11.9. 7. A method for synthesis of Ziegler Nata procatalyst, the method comprising reacting the magnesium alkoxide claimed in any one of the above claims with TiCl and chlorobenzene, the method yielding a reaction side product having the formula

TiClx(OR 1)y(OR2 )z where x, y, z is an integer from 0 to 4 and R1 , R2 is an alkyl or an aryl group, the side product on treatment with a carboxylic acid chloride generates in situ internal donor(s) for the procatalyst. 8. Spheroidal Ziegler Natta procatalyst synthesized by the method as claimed in claim7, the procatalyst having a particle size in the range of 25 to 65 microns and comprising the internal donor(s) generated in situ. 9. The procatalyst as claimed in claim 8 wherein the internal donor(s) is selected from the group consisting of methyl benzoate, ethyl benzoate, n-propyl benzoate, i-propyl

benzoate, n-butyl benzoate, i-butyl benzoate, dimethyl phthalate, diethyl phthalate, dipropyl phthalate, di-isopropyl phthalate, di-butyl phthalate and di-isobutyl phthalate. 10. A method for polymerization of olefin, the method comprising contacting the olefin with a catalyst system comprising a procatalyst as claimed in claim 9, a cocatalyst and optionally a selectivity control agent. 11. Spheroidal polyolefin particles synthesized by the method as claimed in claim 10

ABSTRACT The invention relates to a process for the synthesis of spheroidal magnesium alkoxide having improved mechanical strength and narrow particle size distribution, the process comprising reacting magnesium metal, in the presence of iodine, with a mixture of alcohols by step-wise heating first in the range of 40°C to 65°C for a period of 2 hours and then in the range of 65°C to 80°C for a period of 1 hour, further by maintaining reaction temperature at 80°C for a period of 6 - 10 hours, the vapours of the mixture produced during the reaction being condensed in an overhead condenser, hydrogen gas produced during the reaction being vented off and the mixture of alcohols left after the reaction being filtered and reused. The invention also relates to spheroidal magnesium alkoxide particles synthesized by the method, to the Ziegler natta procatalyst synthesized by using the alkoxide and to the polymer resin synthesised using the procatalyst.

Documents

Sign in to open
Application documents
1 916-MUM-2008-CORRESPONDENCE(17-11-2009).pdf 17 Nov 2009
2 916-MUM-2008-SPECIFICATION(MARKED COPY)-(16-11-2011).pdf 16 Nov 2011
3 916-MUM-2008-SPECIFICATION(AMENDED)-(16-11-2011).pdf 16 Nov 2011
4 916-MUM-2008-REPLY TO HEARING(16-11-2011).pdf 16 Nov 2011
5 916-MUM-2008-CLAIMS(AMENDED)-(16-11-2011).pdf 16 Nov 2011
6 Form 27 [27-03-2017(online)].pdf 27 Mar 2017
7 916-MUM-2008-RELEVANT DOCUMENTS [28-03-2018(online)].pdf 28 Mar 2018
8 916-MUM-2008_EXAMREPORT.pdf 10 Aug 2018
9 916-MUM-2008-REPLY TO EXAMINATION REPORT(25-8-2011).pdf 10 Aug 2018
10 916-MUM-2008-POWER OF ATTORNEY 13-6-2008.pdf 10 Aug 2018
11 916-MUM-2008-MARKED COPY(25-8-2011).pdf 10 Aug 2018
12 916-mum-2008-form-3.pdf 10 Aug 2018
13 916-mum-2008-form-2.pdf 10 Aug 2018
15 916-mum-2008-form-1.pdf 10 Aug 2018
16 916-MUM-2008-FORM 2(TITLE PAGE)-(GRANTED)-(16-3-2012).pdf 10 Aug 2018
17 916-MUM-2008-FORM 2(TITLE PAGE)-(25-8-2011).pdf 10 Aug 2018
18 916-MUM-2008-FORM 2(GRANTED)-(16-3-2012).pdf 10 Aug 2018
19 916-MUM-2008-FORM 18 24-6-2008.pdf 10 Aug 2018
21 916-MUM-2008-FORM 1(26-7-2011).pdf 10 Aug 2018
22 916-MUM-2008-FORM 1 13-6-2008.pdf 10 Aug 2018
23 916-mum-2008-drawings.pdf 10 Aug 2018
24 916-MUM-2008-DRAWING(GRANTED)-(16-3-2012).pdf 10 Aug 2018
25 916-MUM-2008-DESCRIPTION(GRANTED)-(16-3-2012).pdf 10 Aug 2018
26 916-mum-2008-description (complete).pdf 10 Aug 2018
27 916-MUM-2008-CORRESPONDENCE(IPO)-(3-12-2012).pdf 10 Aug 2018
28 916-MUM-2008-CORRESPONDENCE(5-2-2014).pdf 10 Aug 2018
29 916-MUM-2008-CORRESPONDENCE(26-7-2011).pdf 10 Aug 2018
30 916-MUM-2008-CORRESPONDENCE(20-6-2012).pdf 10 Aug 2018
31 916-MUM-2008-CORRESPONDENCE(14-2-2012).pdf 10 Aug 2018
32 916-MUM-2008-CORRESPONDENCE(13-4-2012).pdf 10 Aug 2018
33 916-MUM-2008-CORRESPONDENCE(11-9-2008).pdf 10 Aug 2018
34 916-MUM-2008-CORRESPONDENCE(10-2-2011).pdf 10 Aug 2018
35 916-MUM-2008-CORRESPONDENCE 24-6-2008.pdf 10 Aug 2018
36 916-MUM-2008-CORRESPONDENCE 13-6-2008.pdf 10 Aug 2018
37 916-mum-2008-claims.pdf 10 Aug 2018
39 916-MUM-2008-CLAIMS(GRANTED)-(16-3-2012).pdf 10 Aug 2018
40 916-MUM-2008-CLAIMS(AMENDED)-(25-8-2011).pdf 10 Aug 2018
41 916-MUM-2008-ANNEXURE TO FORM 3(11-9-2008).pdf 10 Aug 2018
42 916-MUM-2008-ANNEXURE TO FORM 3(10-2-2011).pdf 10 Aug 2018
43 916-mum-2008-abstract.pdf 10 Aug 2018
45 916-MUM-2008-ABSTRACT(GRANTED)-(16-3-2012).pdf 10 Aug 2018
46 916-MUM-2008-RELEVANT DOCUMENTS [28-03-2019(online)].pdf 28 Mar 2019
47 916-MUM-2008-RELEVANT DOCUMENTS [30-09-2021(online)].pdf 30 Sep 2021
48 916-MUM-2008-RELEVANT DOCUMENTS [30-09-2022(online)].pdf 30 Sep 2022
49 916-MUM-2008-RELEVANT DOCUMENTS [29-09-2023(online)].pdf 29 Sep 2023
50 916-MUM-2008-FORM-27 [29-09-2026(online)].pdf 29 Sep 2026
51 916-MUM-2008-FORM-27 [29-09-2026(online)]-2.pdf 29 Sep 2026
52 916-MUM-2008-FORM-27 [29-09-2026(online)]-1.pdf 29 Sep 2026

ERegister / renewals

Inforce
3rd Renewed 20 Jun 2012 Period 25 Apr 2010 – 25 Apr 2011 · CBR 8029 · Certificate 3356 ₹2,000
4th Renewed 20 Jun 2012 Period 25 Apr 2011 – 25 Apr 2012 · CBR 8029 · Certificate 3356 ₹2,000
5th Renewed 20 Jun 2012 Period 25 Apr 2012 – 25 Apr 2013 · CBR 8029 · Certificate 3356 ₹2,000
6th Renewed 28 Feb 2013 Period 25 Apr 2013 – 25 Apr 2014 · CBR 2546 · Certificate 1149 ₹2,000
7th Renewed 05 Feb 2014 Period 25 Apr 2014 – 25 Apr 2015 · CBR 1621 · Certificate 719 ₹6,000
8th Renewed 23 Apr 2015 Period 25 Apr 2015 – 25 Apr 2016 · CBR 6464 · Certificate 3395 ₹12,000
9th Renewed 20 Jan 2016 Period 25 Apr 2016 – 25 Apr 2017 · CBR 1135 · Certificate 593 ₹12,000
10th Renewed 19 Apr 2017 Period 25 Apr 2017 – 25 Apr 2018 · CBR 9749 · Certificate 4335 ₹12,000
11th Renewed 19 Apr 2018 Period 25 Apr 2018 – 25 Apr 2019 · CBR 7269 · Certificate 5063 ₹24,000
12th Renewed 15 Apr 2019 Period 25 Apr 2019 – 25 Apr 2020 · CBR 8885 · Certificate 6469 ₹24,000
13th Renewed 20 Mar 2020 Period 25 Apr 2020 – 25 Apr 2021 · CBR 8801 · Certificate 7548 ₹24,000
14th Renewed 30 Mar 2021 Period 25 Apr 2021 – 25 Apr 2022 · CBR 7801 · Certificate 8898 ₹24,000
15th Renewed 05 Jan 2022 Period 25 Apr 2022 – 25 Apr 2023 · CBR 352 · Certificate 509 ₹24,000
16th Renewed 31 May 2022 Period 25 Apr 2023 – 25 Apr 2024 · CBR 14028 · Certificate 15608 ₹40,000
17th Renewed 22 Apr 2024 Period 25 Apr 2024 – 25 Apr 2025 · CBR 19787 · Certificate 47811 ₹40,000
18th Renewed 03 Apr 2025 Period 25 Apr 2025 – 25 Apr 2026 · CBR 13267 · Certificate 15415 ₹40,000
19th Renewed 09 Apr 2026 Period 25 Apr 2026 – 25 Apr 2027 · CBR 15399 · Certificate 16398 ₹40,000